The froth is skimmed off and the resulting lead sulphide concentrate is dried. During this process, the ore, which may contain only 5% lead, is upgraded to a concentrate with 50% or more lead. At Broken Hill, concentrate grades average about 70% lead, mainly because the relatively coarse grain of the ore allows excellent recovery of lead sulphides.