The cold pilgering test is performed using a typical 75VMR- After type mill manufactured by Meer, the roll die diameter of Extrusion which is 370 mm, and the working-zone length is 750 mm. The flaw detection of the cold-pilgered tube is performed by ultrasonic testing, penetration testing, and visual inspection. 3. Results