Potash Flotation Process
Hammer mills can generally be set to dry crush to 95% — 10M. Scrubbing and Desliming The dry crushed ore at minus 6 mesh is fed into a rotary drum scrubber with saturated salt brine. The action in the scrubber scours off the surface film of clay slime from the salt crystals.